Cryogenic drilling of KevlarTM composite laminates
| dc.contributor.author | MUJAHED AHMED | |
| dc.date | 2004 | |
| dc.date.accessioned | 2022-05-18T06:11:15Z | |
| dc.date.available | 2022-05-18T06:11:15Z | |
| dc.degree.department | College of Engineering Sciences and Applied Engineering | |
| dc.degree.grantor | King Fahad for Petrolem University | |
| dc.description.abstract | ﻟﻘﺪ ازدادت أهﻤﻴﺔ اﻟﻤﻜﺎﺋﻦ اﻟﻠﺘﻲ ﺗﻌﻤﻞ ﺑﺎﻟﺘﺒﺮﻳﺪ ﻓﻲ اﻟﺼﻨﺎﻋﺎت اﻟﻤﻌﺪﻧﻴﺔ وﺑﺪأت ﺗﺤﻞ ﻣﺤﻞ اﻟﻤﻜﺎﺋﻦ اﻟﺘﻘﻠﻴﺪﻳﺔ ﻟﻠﺘﻐﻠﺐ ﻋﻠﻰ ﻋﻴﻮب اﻟﻤﺒﺮدات اﻟﺘﻘﻠﻴﺪﻳﺔ . إن ﻣﻮاد ﻣﺜﻞ ﻓﺎﻳﺒﺮ اﻷراﻣﻴﺪ اﻟﻤﺮآﺐ واﻟﻤﺪﻋﻢ ﻣﻦ اﻟﺼﻌﻮﺑﺔ ﺑﻤﻜﺎن أن ﺗﺼﻨﻊ ﺑﺴﺒﺐ اﻟﺨﻮاص اﻟﻔﺮﻳﺪة اﻟﻤﻤﺜﻠﺔ ﻓﻲ اﻟﺼﻔﺎت اﻟﻔﻴﺰﻳ ﺗﺮآﻴﺒﻪ ﺎﺋﻴﺔ ﻟﻜﻞ ﻣﻦ اﻟﻔﺎﻳﺒﺮ واﻟﻤﻜﻮﻧﺎت اﻟﺪاﺧﻠﺔ ﻓﻲ . إن اﻟﺪراﺳﺔ اﻟﺤﺎﻟﻴﺔ Kevlar ﺗﻘﻴﻢ ﺗﺼﻨﻴﻊ TM-49 .TiN coated HSS drill اﻟﻤﺮآﺐ ﻣﻦ ﺻﻔﺎﺋﺢ ﻋﻨﺪ درﺟﺔ ﺣﺮارة ﻣﻨﺨﻔﻀﺔ ﺑﺎﺳﺘﺨﺪام ﻋ ، ﺗﻢ ﺗﻘﻴﻴﻢ ﺗﺄﺛﻴﺮ آﻞ ﻣﻦ درﺟﺔ اﻟﺤﺮارة و ﻇﺮوف اﻟﻘﻄﻊ ﻋﻤﻠﻴﺔ ﺗﺼﻨﻴﻊ اﻟﺼﻔﺎﺋﺢ ﻋﻦ ﻃﺮﻳﻖ ﻗﻮة اﻟﺤﻔﺮ اﻟﺪﻓﻌﻲ ﺰم . اﻟﻄﺎﻗﺔ اﻟﻔﻌﺎﻟﺔ و ﺟﻮدة اﻟﺜﻘﺐ ، اﻟﻘﻄﻊ وﻟﻘﺪ وﺟﺪ إن آﻼ ﻣﻦ ﺣﺮارة اﻟﻘﻄﻌﺔ اﻟﻤﺸﻐﻮﻟﺔ و ﻇﺮوف اﻟﺘﺼﻨﻴﻊ ﺗﺆﺛﺮ ﻋﻠﻰ آﻞ . ﻃﺎﻗﺔ اﻟﻘﻄﻊ اﻟﻔﻌﺎﻟﺔ ﺑﻤﺴﺘﻮﻳﺎت ﻣﺘﻔﺎوﺗﺔ ، اﻟﻌﺰم اﻷﻗﺼﻰ ، ﻣﻦ اﻟﻘﻮة اﻟﺪﻓﻌﻴﺔ اﻟﻘﺼﻮى ﺗﻢ اﺧﺘﺒﺎر اﻟﻔﺮﺿﻴﺔ ﻟﺪراﺳﺔ ﺗﺄﺛﻴﺮ ﺧﻔﺾ ﺣﺮارة اﻟﻘﻄﻌﺔ اﻟﻤﺸﻐﻮﻟﺔ ﻋﻠﻰ ﻗﻮة اﻟﺘﺼﻨ اﻟﺜﻘﺐ ﻴﻊ و ﺟﻮدة . وﻟﻘﺪ أﻇﻬﺮ آﻼ ﻣﻦ اﻟﺤﻔﺮ اﻟﺪﻓﻌﻲ و اﻟﻌﺰم زﻳﺎدة ﻃﺮدﻳﺔ ﻣﻊ ﺧﻔﺾ ﺣﺮارة اﻟﻘﻄﻌﺔ اﻟﻤﺸﻐﻮﻟﺔ ﺑﺴﺒﺐ هﺸﺎﺷﺔ اﻟﺼﻔﺎﺋﺢ ﻋﻨﺪ درﺟﺎت اﻟﺤﺮارة اﻟﻤﻨﺨﻔﻀﺔ . وﻟﻘﺪ أﻇﻬﺮت اﻟﺜﻘﻮب اﻟﻤﺤﻔﻮرة ﻟﻠﺼﻔﺎﺋﺢ واﻟﻠﺘﻲ ﺗﻢ اﻟﺤﺼﻮل ﻋﻠﻴﻬﺎ ﺑﺎﻟﺘﻘﻨﻴﺎت اﻟﺒﺼﺮﻳﺔ وﺟﻮد ﻧﺘﻮءات وﺗﺸﻘﻘﺎت أﻗﻞ ﻟﻠﺼﻔﺎﺋﺢ ﻋﻨﺪ درﺟﺎت ﺣﺮارة ﻣﻨﺨﻔﻀﺔ ﻣﻘﺎرﻧﺔ ﻣﻊ درﺟﺔ اﻟﻤﺤﻴﻂ اﻟﻌﺎدﻳﺔ . 400% وﺗﻢ ﻣﻼﺣﻈﺔ ﺗﺤﺴﻦ ﻣﻘﺪارﻩ ﻋﻨﺪﻣﺎ ﺗﻢ ﺧﻔﺾ درﺟﺔ اﻟﻐﺮﻓﺔ 120 اﻟﺤﻠﺮارة اﻟﻤﺸﻐﻮﻟﺔ إﻟﻰ درﺟﺔ ﻣﺌﻮﻳﺔ ﺗﺤﺖ اﻟﺼﻔﺮ ﻣﻘﺎرﻧﺔ | |
| dc.identifier.other | 4214 | |
| dc.identifier.uri | https://drepo.sdl.edu.sa/handle/20.500.14154/2204 | |
| dc.language.iso | en | |
| dc.publisher | Saudi Digital Library | |
| dc.thesis.level | Master | |
| dc.thesis.source | King Fahad for Petrolem University | |
| dc.title | Cryogenic drilling of KevlarTM composite laminates | |
| dc.type | Thesis |